AbstractThe compatibility of 04X16H11M3T austenitic steel and 05X12H2M ferrite-martensite steel with eutectic 17Li-83Pb at 773, 673 and 593 K and circulation with 0.5 and 1.5 m/s velocities has been investigated. The experiment time was 3000 hours. The 04X16H11M3T steel specimens have been investigated both in unstressed and stressed conditions.As a result of investigations the porous ferritic layer was not detected in 04X16H11M3T steel specimens.The significant effect of eutectic velocity on structural materials corrosion resistance has been shown. The stressed conditions results in increase in mass losses from 04X16H11M3T steel specimens.The 04X16H11M3T steel can be used for operation with eutectic 17Li-83Pb at velocities up to 1.5 m/s and temperatures up to 627 K.
抽象 04X16H11M3Tオーステナイト鋼と05X12H2Mフェライト・マルテンサイト鋼の、共晶17Li-83Pbに対する耐食性を、773K、673K、593Kの温度で、流速0.5m/s、1.5m/s、2.5m/sの条件下で調査した。実験は3000時間実施した。その結果、04X16H11M3T鋼は、流速1.5m/s、温度627Kまでの条件下で共晶17Li-83Pbとの併用に適していることが示された。05X12H2M鋼は、試験したすべての条件下で、共晶17Li-83Pb中での使用には適さない。04X16H11M3T鋼の耐食性は、鋼表面への共晶成分の移行と、その後の緻密で強固な保護層の形成によって確保される。05X12H2M鋼では、多孔質で密着性の低い層が形成される。04X16H11M3T鋼の試験片は、応力を受けた状態と応力を受けていない状態の両方で調査された。応力を受けた状態では、応力を受けていない状態と比較して、質量損失の増加は観察されなかった。調査の結果、多孔質のフェライト層は04X16H11M3T鋼の試験片では検出されなかった。共晶17Li-83Pb中での04X16H11M3T鋼の使用は、流速1.5m/sまで、温度627Kまで可能である。