AbstractTo obtain further information on the transient permeation behavior of hydrogen isotopes as caused by an abrupt temperature change, numerical calculations were carried out for two typical metals, nickel and vanadium.Deuterium permeation through nickel is analyzed as a typical case of bulk-diffusion-limited permeation. Its transient behavior changed dramatically according to the specimen thickness. The transient behavior, in general, is separated into two parts, initial and latter period behaviors. Conditions which cause such a separation were evaluated. Evaluation of the hydrogen diffusivity and solubility by an analysis of transient curves of hydrogen permeation was carried out.The transient behavior of simultaneous gas- and ion-driven hydrogen permeation through vanadium was also analyzed. Overshooting of the hydrogen permeation rate appears with an abrupt temperature increase. Increasing the impinging ion flux causes the overshooting peak to become sharper, and also reduces the change of the steady-state permeation rate to be attained after the temperature change compared with the initial value.
要約 水素同位体の過渡透過挙動に関するさらなる知見を得るため、急激な温度変化によって引き起こされる現象について、ニッケルとバナジウムという2つの代表的な金属に対して数値計算を実施した。 ニッケルを透過する重水素は、バルク拡散律速透過の典型的なケースとして解析された。その過渡挙動は、試験片の厚さに応じて劇的に変化した。過渡挙動は、一般的に、初期期間と後期期間の2つの部分に分けられる。このような分離を引き起こす条件が評価された。水素透過曲線の過渡解析による水素拡散係数と溶解度の評価が実施された。 バナジウムを透過する同時ガス駆動およびイオン駆動水素の過渡挙動も解析された。水素透過速度のオーバーシュートは、急激な温度上昇とともに現れる。入射イオンフラックスの増加は、オーバーシュートピークをより鋭くし、また、初期値と比較した場合の温度変化後に達成される定常透過速度の変化を低減させる。