AbstractWe measured the frequency characteristics of ac losses in the aluminum-stabilized superconducting conductor for the helical coil system of the Large Helical Device (LHD) project, in order to clarify the dependence of the loss on the sweep rate of the poloidal field. In our experiment, a straight and short conductor of about 50 cm long was used as a sample. The sample was subjected to the ac ripple field superposed on the bias field. The data of the ac loss observed in the frequency range from 0.1 to 100 Hz have two peaks just as our analysis predicted. The peak at the lower frequency is the critical frequency related to the inter-strand coupling time constant τc. The other peak at the higher frequency is the skin frequency of the normal metal around the strand bundle in the conductor. The lower frequency peak mainly shifts according to the cabling condition of the strand bundle. Under the operating condition of the LHD corresponding to 0.1 Hz, the loss can be decreased as τc increases. It is very different from the common design concept. This result suggests that it is necessary to grasp the sweep-rate dependence of the loss in the conductor in order to optimize its structure from the low-loss point of view.
我々は、LHD計画のヘリカルコイルシステム用アルミ安定化超伝導導体における交流損失の周波数特性を測定し、ポロイダル磁場の掃引速度に対する損失の依存性を明らかにすることを目的とした。実験では、約50cmの短尺直線導体を試料として用いた。試料には、バイアス磁場に重畳して交流リップル磁場を印加した。0.1Hzから100Hzの周波数範囲で観測された交流損失のデータは、我々の解析が予測したとおり、2つのピークを示した。低周波側のピークは、ストランド間結合時定数τcに関連する臨界周波数に対応する。高周波側のピークは、導体内のストランド束周囲の常伝導金属における表皮周波数に対応する。低周波側のピークは、ストランド束のケーブル化条件に主に依存してシフトする。LHDの運転条件に相当する0.1Hzでは、τcを増加させることで損失を低減できる。これは一般的な設計概念とは大きく異なる。この結果は、低損失の観点から導体構造を最適化するためには、導体における損失の掃引速度依存性を把握することが必要であることを示唆している。